Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 6.90 - 12.1 MPa | 1000 - 1750 psi | |
Pyrotek SF-50 Foamed Fused Silica Insulation Board SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o.. |