Polymer Property : Compressive Strength = 59.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 59.0 MPa
8560 psi
Pyrotek F-51 Dense Machinable Board
F-51 is a high temperature resin base, supplemented with fiberglass and graphite to provide extra strength and lubricity. F-51 is abrasion resistant and suitable for hot glass handling applications..
Compressive Strength 59.0 MPa

@Time 36.0 sec
8560 psi

@Time 0.0100 hour
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified
Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn..