Polymer Property : Compressive Strength = 573.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 573.9 MPa
83230 psi
Warp; D 6641-01
Ensinger TECATEC™ CF60 Polyaryletherketone (PAEK)
TECATEC™ CF60 plate is a composite of 60% woven carbon fiber laminated with a polyaryl ether ketone resin (PAEK). It is produced in a proprietary process yielding good fibre and resin integration...