Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 56.5 MPa | 8200 psi | ASTM D-695 |
CMT Materials REN Shape® 5008 Vacuum Forming Tooling Board REN SHAPE 5008 is a tooling board specifically designed for use in vacuum forming. It is designed for use up to 250°F and is well suited for building vacuum forming molds as well as master models,.. |
|||
Compressive Strength | 56.5 MPa | 8200 psi | |
Aremco Ceramacast™ 895 High Temperature Potting & Casting Material Alumina Fine grain castable ceramic. |