Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 324 MPa @Temperature 23.9 °C |
47000 psi @Temperature 75.0 °F |
Dry; 325°F Autoclave; ASTM D695 |
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Commercial Silica Fabric Reinforced Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz.. |
|||
Compressive Strength | 324 MPa | 47000 psi | Open Hole |
Greene Tweed Xycomp® 1001-01 PEEK, Carbon Fiber Filled Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st.. |