Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 44.8 MPa | 6500 psi | Ultimate; Mixed 1:1; TM R050-38 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Compressive Strength | 44.8 MPa | 6500 psi | Break; Mixed 1:1; TM R050-38 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Compressive Strength | 44.8 MPa | 6500 psi | |
Trelleborg AEM Syntac® 350 Syntactic Foam Syntac® 350 is made from high grade epoxy resin and hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling.Available in block, sheet and ro.. |
|||
Compressive Strength | 44.8 MPa | 6500 psi | |
Trelleborg AEM Syntac® 351 Syntactic Foam Syntac® 351 is a castable syntactic composite material of epoxy resin and high performance hollow glass microspheres designed specifically for molding thermoforming plugs and other associated tooli.. |
|||
Compressive Strength | 44.8 MPa | 6500 psi | |
Trelleborg Emerson & Cuming Syntac® 350 Composite Materials Syntactic Foam Syntac 350 foam is a rigid, high strength composite of epoxy resin and microscopic hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling. .. |
|||
Compressive Strength | 44.8 MPa | 6500 psi | Ultimate; TM R050-38 |
Resinlab® EP1200 Black Casting Resin Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re.. |
|||
Compressive Strength | 44.8 MPa | 6500 psi | Ultimate; TM R050-38 |
Resinlab® EP1200LV Casting Resin Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an.. |
|||
Compressive Strength | 44.8 - 48.3 MPa | 6500 - 7000 psi | Ultimate; TM R050-38 |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |