Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 44.1 MPa | 6400 psi | Cold Crushing |
Sharadaa Ceramics LI SILL-II High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | 44.1 MPa | 6400 psi | Cold Crushing Strength |
Chosun Refractories H-3 High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 44.1 MPa | 6400 psi | Cold Crushing Strength |
Chosun Refractories CH-1 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 44.1 MPa | 6400 psi | Cold Crushing Strength |
Chosun Refractories PCB-50 Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 44.1 MPa | 6400 psi | Cold Crushing Strength |
Chosun Refractories PCB-TB Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 44.1 MPa | 6400 psi | Cold Crushing Strength |
Chosun Refractories H-4S High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |