Chosun Refractories PCB-TB Casting Block

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories PCB-TB Casting Block.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.40 g/cc
0.0867 lb/in³
Porosity 13 %
13 %
Mechanical Properties Metric English Comments
Compressive Strength 44.1 MPa
6400 psi
Cold Crushing Strength
Component Elements Properties Metric English Comments
Al2O3 50 %
50 %
SiO2 46 %
46 %
Descriptive Properties Value Comments
Characteristics & Main Applications Spaling Resistance Tank Block