Polymer Property : Compressive Strength = 43500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength >= 300 MPa
>= 43500 psi
Normal to Plane; EN ISO 604
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite
Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o..
Compressive Strength 300 MPa
43500 psi
Sapco C 410 Steatite
Information provided by Sapco.
Compressive Strength 300 MPa
43500 psi
ISO 604
Vyncolit X655 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask..
Compressive Strength 300 MPa
43500 psi
Longitudinal
Goodfellow E-glass/Epoxy Composite
Boro-silicate glass/EpoxyInformation provided by Goodfellow.
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit I Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity.Application: Insulation material in hig..
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit II Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Mechanical and electrical applications used at normal air humidity. Very good electrical values.Information provided by Elektro-Isola
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit IIQ R Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit IIQ R XX Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit IR Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity. Very low water absorption.Application:..
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit IS Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Very good high-voltage insulation material. Very high breakdown voltage, in particular parallel to the layers. Dimensionally stable.Application: Insulation material in high-voltage tap ..
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected and lasting electrical properties despit..
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit IV Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected. Suitable as high-frequency insulation o..
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart..
Compressive Strength 300 MPa

@Temperature 23.0 °C,
Time 86400 sec
43500 psi

@Temperature 73.4 °F,
Time 24.0 hour
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Tubes
Description: Extremely good mechanical properties, at high temperatures. Low thermal conductivity.Applications: Material for components used in the aerospace industry. Insulation parts in wire weldi..
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m..
Compressive Strength 300 MPa

@Treatment Temp. 20.0 °C,
Time 3600 sec
43500 psi

@Treatment Temp. 68.0 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m..
Compressive Strength 300 MPa

@Temperature 23.0 °C
43500 psi

@Temperature 73.4 °F
Elisto THERMOSTAR® MD 150 Pattern material
Industrial laminateInformation provided by elisto
Compressive Strength >= 300 MPa
>= 43500 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet
Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions.Information..
Compressive Strength >= 300 MPa
>= 43500 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe PF CP 202 Cellulose Paper Reinforced Phenolic Resin - Sheet
High voltage applications at power frequencies. High electric strength under oil. Good electrical strength in air under normal humidity.Information provided by Hippe.
Compressive Strength >= 300 MPa
>= 43500 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe PF CP 207 Cellulose Paper Reinforced Phenolic Resin - Sheet
Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions. Improved ..
Compressive Strength >= 300 MPa
>= 43500 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe PF CP 308 Cellulose Paper Reinforced Phenolic Resin - Sheet
Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions. Flame retardant.Information provided by Hippe.
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T..
Compressive Strength 300 MPa
43500 psi
EN ISO 604
Brandenburger BL 20/1 GG EP Rotor Blade Material
BL 20/1 GG EP is a composite bearing material that combines the crucial parameters for rotary blades. These include compressive stability at high temperatures, impact strength, low swelling and low..
Compressive Strength 300 - 400 MPa
43500 - 58000 psi
Alliance A-5S Alnico Magnetic Material
Compressive Strength 300 - 400 MPa
43500 - 58000 psi
Alliance A-8S Alnico Magnetic Material
Compressive Strength 300 - 400 MPa
43500 - 58000 psi
Alliance A-6S Alnico Magnetic Material
Compressive Strength 300 - 400 MPa
43500 - 58000 psi
Alliance A-2S Alnico Magnetic Material