Category Polymer , Thermoset , Phenolic , Phenolic, Novolac, Cellulose Filled
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PF CP 207 Cellulose Paper Reinforced Phenolic Resin - Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions. Improved punching characteristics at lower temperature when compared to PF CP 201Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.40 g/cc
1.30 - 1.40 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 100 MPa
>= 14500 psi
IEC 1212-2 5.7
Flexural Strength >= 80.0 MPa
>= 11600 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 5.00 GPa
>= 725 ksi
IEC 1212-2 5.2
Compressive Strength >= 300 MPa
>= 43500 psi
Perpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 10.0 MPa
>= 1450 psi
Parallel to laminations; IEC 1212-2 5.6
Electrical Properties Metric English Comments
Comparative Tracking Index >= 100 V
>= 100 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Thermal Endurance 105 T.I.
IEC 1212-2 7.1
Water Absorption < 920 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm