Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2.90 MPa | 421 psi | Dried at 110°C (230°F) |
Skamol Group SKAMOCAST 112-80 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |