Mechanical Properties Metric English Comments
Compressive Strength 40.0 MPa
5800 psi
10% Def.; ASTM D695
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet)
KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re..
Compressive Strength 40.0 MPa

@Time 3.60e+7 sec
5800 psi

@Time 10000 hour
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex
Compressive Strength 40.0 MPa
5800 psi
ASTM-C773
CoorsTek PolyGlyde™ 2000 Self-Lubricating Seal
PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni..
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Chosun Refractories A12HM Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Chosun Refractories A12S Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Chosun Refractories C15A Magnesia Carbon Brick for Converter
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength >= 40.0 MPa
>= 5800 psi
Axial; IEC 1212-2 4.2
Hippe SI GC 21 Woven Glass Cloth Reinforced Silicone Resin - Round, Rolled Tube
Good mechanical, electrical and electronic applications when exposed to high relative humidity.Information provided by Hippe.
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Chosun Refractories L12H Magnesia Carbon Bricks for Ladle Slag Line
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Chosun Refractories L12HU Magnesia Carbon Bricks for Ladle Slag Line
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Chosun Refractories L12S Magnesia Carbon Bricks for Ladle Slag Line
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Chosun Refractories L15H Magnesia Carbon Bricks for Ladle Slag Line
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Chosun Refractories L15HU Magnesia Carbon Bricks for Ladle Slag Line
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Chosun Refractories L15S Magnesia Carbon Bricks for Ladle Slag Line
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength >= 40.0 MPa
>= 5800 psi
Ambient
China-Yixing Longly Refractories ASM-130 Cordierite-Mullite
Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b..
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Chosun Refractories A12H Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).