Polymer Property : Compressive Strength = 3980 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 27.5 MPa
3980 psi
Cold Crushing Strength
Chosun Refractories CRAG-L15 Shroud Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 27.5 MPa
3980 psi
Cold Crushing Strength
Chosun Refractories CRAG-L44 Shroud Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).