Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 27.5 MPa | 3980 psi | Cold Crushing Strength |
Chosun Refractories CRAG-L15 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 27.5 MPa | 3980 psi | Cold Crushing Strength |
Chosun Refractories CRAG-L44 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |