Polymer Property : Compressive Strength = 3400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 23.4 MPa
3400 psi
10% Def.; ASTM D695
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet)
Compressive Strength 23.4 MPa
3400 psi
10% Def.; ASTM D695
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)  (Unverified Data**)
Compressive Strength 23.4 MPa
3400 psi
ASTM D695
Greene Tweed Avalon® 9 PTFE, Graphite Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
Compressive Strength 23.4 MPa
3400 psi
1% strain; ASTM D695
Saint-Gobain Meldin® 7021 Direct Formed Graphite Filled Polyimide
Finished parts and basic shapes made from 15% by weight graphite filled polyimide material for applications high wear resistance, good thermal oxidative stability, and high temperature resistance. ..