Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.230 MPa | 33.4 psi | non-fired at 10% compressions |
Pyrotek Pyrotherm TF-19 Lightweight, non-RCF insulation board for ovens, furnaces, kilns and vessels Pyrotherm TF-19 is a high-temperature board providing high strength and excellent workability. It is composed of mineral fiber and selected mineral additives.ApplicationsPot cradle insulation (for .. |