Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek Pyrotherm TF-19 Lightweight, non-RCF insulation board for ovens, furnaces, kilns and vessels

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name Pyrotherm
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyrotherm TF-19 Lightweight, non-RCF insulation board for ovens, furnaces, kilns and vessels.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pyrotherm TF-19 is a high-temperature board providing high strength and excellent workability. It is composed of mineral fiber and selected mineral additives.ApplicationsPot cradle insulation (for Alcoa A-697 pots) Precipitators Dryers Ducts and breeching Utility boilers Furnaces Kilns AdvantagesExcellent mechanical strength in non-fired condition Refractory ceramic fiber free Low thermal conductivity Use of large-size boards to reduce labor costs Material can be cut quickly by hand with knife or saw for fabrication and application on the job Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.296 g/cc
0.0107 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000660 GPa
0.0957 ksi
Compressive Strength 0.230 MPa
33.4 psi
non-fired at 10% compressions
Thermal Properties Metric English Comments
Thermal Conductivity 0.0700 W/m-K

@Temperature 260 °C
0.486 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.0900 W/m-K

@Temperature 371 °C
0.625 BTU-in/hr-ft²-°F

@Temperature 700 °F
0.120 W/m-K

@Temperature 482 °C
0.833 BTU-in/hr-ft²-°F

@Temperature 900 °F
Maximum Service Temperature, Air 1038 °C
1900 °F
Shrinkage <= 2.50 %

@Temperature 1038 °C,
Time 86400 sec
<= 2.50 %

@Temperature 1900 °F,
Time 24.0 hour
Copyright © lookpolymers.com All Rights Reserved