Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 22.1 MPa | 3200 psi | 1% strain; ASTM D695 |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Compressive Strength | 22.1 MPa | 3200 psi | |
Engineered Syntactic Systems MZ-24 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |
|||
Compressive Strength | 22.1 MPa | 3200 psi | |
Cotronics Resbond™ 905 High Temperature Ceramic Adhesive, Low Expansion |
|||
Compressive Strength | >= 22.1 MPa | >= 3200 psi | ASTM D365 |
Touchstone CFOAM® 30 Structural Carbon Foam CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins.. |