Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 320 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 320 MPa
46400 psi
ISO 604
Schwartz Technical Plastics MITELA® 2/5 A Cotton Fabric, Special Quality
Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 320 MPa
46400 psi
ISO 604
Schwartz Technical Plastics MITELA® HD8B Cotton Fabric, Special Quality
Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 320 MPa
46400 psi
ISO 604
Sumitomo Bakelite North America CF 9040A Carbon Fiber Reinforced Phenolic
CF 9040A is a high strength carbon fiber phenolic molding compoundInformation provided by Sumitomo Bak North America, Inc.
Compressive Strength 320 MPa

@Thickness >=5.00 mm
46400 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets
Description: Exclusively for mechanical applications. Impact-resistant, resistant to mechanical wear, noise-reducing, low friction. Well suited for parts where there are high mechanical load and wea..
Compressive Strength 320 MPa

@Thickness >=5.00 mm
46400 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronax MFP G Phenolic, Cotton/synthetic Fabric Reinforcement, Black, Sheets
Description: Exclusively for mechanical applications. The combination of cotton/synthetic reinforcement and a graphite-modified resin results in a material with low friction and especially high wear..
Compressive Strength 320 MPa

@Thickness >=5.00 mm
46400 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit AS Phenolic, Paper Reinforcement, Black, Sheets
Description: ESD-protection quality according to SP-method 2472, IEC 61340-5-1 and EN 100015-1. SP ESD Approval Certificate No. 230-01-0137. High mechanical properties at temperatures up to 120°CAp..
Compressive Strength 320 MPa

@Thickness >=5.00 mm
46400 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit IIQ Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Compressive Strength 320 MPa

@Thickness >=5.00 mm
46400 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit IIQ S AL Phenolic, Paper Reinforcement, Black with foil, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good ..
Compressive Strength 320 MPa

@Thickness >=5.00 mm
46400 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronit IIQ S Phenolic, Paper Reinforcement, Black, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good ..
Compressive Strength 320 MPa

@Treatment Temp. 100 °C,
Time 3600 sec
46400 psi

@Treatment Temp. 212 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets
Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope..
Copyright © lookpolymers.com All Rights Reserved