Polymer Property : Compressive Strength = 31300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 216 MPa
31300 psi
ASTM D695
Plenco 7021 Phenolic, Granular, Injection Molded
PLENCO 07021 is a renumber of Plaslok 7021 which is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compressio..