Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 21.0 MPa | 3050 psi | 35-45% |
Pyrotek Firefly 800 Roller & Furnace Cladding Material Firefly 800 is a beige asbestos-free material made from high-quality shot-free mineral wool and inert fillers. Rollers made of Firefly 800 are constructed to resist breakage in handling service. F.. |
|||
Compressive Strength | 21.0 MPa | 3050 psi | 0.42 |
Pyrotek U-1 Compressible Board U-1 is a high-temperature millboard that is easily cut, punched and shaped. It works well as a roll-cladding material and as compressible gasketing. A unique characteristic of the asbestos-free bo.. |
|||
Compressive Strength | 21.0 MPa | 3050 psi | 5% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 21.0 MPa | 3050 psi | 5% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Dry Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 21.0 MPa | 3050 psi | ASTM D695 |
BCC Products LIK-WOOD BC 8007 Urethane Casting Lik-Wood is a low viscosity, quick setting, easy to use casting material. A model or tool cast from Lik-Wood will weigh 60% less than other filled urethane systems. Within 30 minutes after mixing an.. |