Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 203 MPa @Thickness 12.7 mm |
29500 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP625 Paper Base Laminate Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611. |
|||
Compressive Strength | 203 MPa | 29500 psi | |
SGL Carbon Group Ridurid® V 1352 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |