Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 167 MPa | 24200 psi | |
Ohio Carbon Blank OCB AR-14 EDM Grade Graphite Available in a range of sizes and shapes. |
|||
Compressive Strength | 167 MPa | 24200 psi | ASTM D695 |
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Compressive Strength | 167 MPa | 24200 psi | ASTM D695 |
Ensinger Tecapeek® XP-103 Compression Molded PEEK Compound, 15% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |