Ensinger Tecapeek® XP-103 Compression Molded PEEK Compound, 15% Carbon Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-103 Compression Molded PEEK Compound, 15% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Filler Content 15 %
15 %
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 104
104
ASTM D785
Hardness, Shore D 88
88
ASTM D2240
Tensile Strength 106 MPa
15400 psi
ASTM D638
Elongation at Break 2.8 %
2.8 %
ASTM D638
3.3 %
3.3 %
Flexural Strain; ASTM D790
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Flexural Strength 203 MPa
29500 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Compressive Strength 167 MPa
24200 psi
ASTM D695
Compressive Modulus 3.45 GPa
500 ksi
ASTM D695
Izod Impact, Notched 0.342 J/cm
0.640 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 34.2 µm/m-°C
19.0 µin/in-°F
ASTM E831
Melting Point 343 °C
649 °F
DSC
Heat Distortion Temperature 253 °C
487 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance <= 10000 ohm
<= 10000 ohm
ASTM D257
Descriptive Properties Value Comments
Color Black