Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 24.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 24.8 MPa
3600 psi
10% Def.; ASTM D695
Quadrant EPP TIVAR® Polysteel Filled UHMW-PE, High Specific Gravity (ASTM Product Data Sheet)
Compressive Strength 24.8 MPa

@Strain 1.00 %
3600 psi

@Strain 1.00 %
ASTM D695
Saint-Gobain Meldin® 7003 Isostatically Molded Bearing Grade MoS2 Filled Polyimide
Melidin® 7003 is a thermosetting polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions. Meldin® 700..
Copyright © lookpolymers.com All Rights Reserved