Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Meldin® 7003 Isostatically Molded Bearing Grade MoS2 Filled Polyimide

Category Polymer , Thermoset , Polyimide, TS
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Meldin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Meldin® 7003 Isostatically Molded Bearing Grade MoS2 Filled Polyimide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melidin® 7003 is a thermosetting polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions. Meldin® 7000 series materials exhibit extremely high geometric stability at elevated temperatures.Specification Qualifications:Satisfies Type III, Class M for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide ResinSatisfies Class 5, Form M for SAE AMS 3644G: Polyimide, Molded Rod, Bar and Tube, Plaque, and Formed PartsSatisfies Type III, Class M for MIL-R-46198: Resin, Polyimide, Hot Pressed or Pressed and Sintered
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ASTM D792
Water Absorption 0.24 %

@Time 86400 sec
0.24 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell E 46
46
ASTM D785
Tensile Strength 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Strength 93.8 MPa
13600 psi
ASTM D790
Flexural Modulus 3.60 GPa
522 ksi
ASTM D790
Compressive Strength 41.4 MPa
6000 psi
0.1% Offset; ASTM D695
24.8 MPa

@Strain 1.00 %
3600 psi

@Strain 1.00 %
ASTM D695
124 MPa

@Strain 10.0 %
18000 psi

@Strain 10.0 %
ASTM D695
Compressive Modulus 2.50 GPa
363 ksi
ASTM D695
Thermal Properties Metric English Comments
CTE, linear 51.7 µm/m-°C

@Temperature 23.9 - 260 °C
28.7 µin/in-°F

@Temperature 75.0 - 500 °F
ASTM E831