Polymer Property : Compressive Strength = 22600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 128 - 156 MPa
18600 - 22600 psi
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound
BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av..