Polymer Property : Compressive Strength = 2210 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 2210 MPa
321000 psi
HRC 62 R<sub>c</sub>0.2.
Assab Steels ASSAB XW-5 Cold Work Steel
ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:High wear resistanceHigh compressive strengthHigh surface hardness after hardeningGood through-hardening..
Compressive Strength 2210 MPa
320000 psi
62 HRC
Schmolz + Bickenbach Cryodur® 2363 (A-2) Cold Work Die Steel
Description: Cryodur® 2363 is a cold-work steel developed for an excellent combination of wear resistance and toughness and Supplied in the annealed conditionCharacteristics: Good wear resistance; ..
Compressive Strength 2210 MPa
320000 psi
62 HRC
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel
Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;..
Compressive Strength 2210 MPa
320000 psi
62 HRC
Schmolz + Bickenbach Cryodur® 2510 (O-1) Cold Work Die Steel
Description: Cyrodur ® 2510 is a single melt Extra Fine Structure (EFS) material; and Supplied in the soft annealed conditionCharacteristics: Excellent dimensional stability during heat treatment; ..