Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1520 MPa | 220000 psi | |
Materion FormaMet, EquaCast® Aluminium Bronze Cold Working Die Alloy FormaMet is an aluminum bronze cold working die alloy used for the drawing or forming of stainless steel, low carbon steel and other materials. When used for deep drawing and forming applications of.. |