Materion FormaMet, EquaCast® Aluminium Bronze Cold Working Die Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name FormaMet, EquaCast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion FormaMet, EquaCast® Aluminium Bronze Cold Working Die Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormaMet is an aluminum bronze cold working die alloy used for the drawing or forming of stainless steel, low carbon steel and other materials. When used for deep drawing and forming applications offer the following advantages:39 HRc hardness minimizes wear and maximizes tool lifeHigh galling resistance eliminates wrinkling and tearing of the deep drawn partVery high wear resistance combined with excellent sliding propertiesInformation supplied by Brush Wellman Engineered Materials.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 6.95 g/cc
0.251 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 39
39
Elongation at Break <= 0.5 %
<= 0.5 %
Compressive Strength 1520 MPa
220000 psi
Thermal Properties Metric English Comments
Thermal Conductivity 38.0 W/m-K
264 BTU-in/hr-ft²-°F