Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 15.0 MPa | 2180 psi | 1% strain over 1000 hours; ISO.899 DIN.53444 |
Omnia Plastica Rilsan® PA6 GF - Akulon GF - at 50% RH Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitabl.. |
|||
Compressive Strength | 15.0 MPa @Time 36.0 sec |
2180 psi @Time 0.0100 hour |
|
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Compressive Strength | 15.0 MPa @Strain 3.50 % |
2180 psi @Strain 3.50 % |
DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Compressive Strength | 15.0 MPa @Time 36.0 sec |
2180 psi @Time 0.0100 hour |
|
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Compressive Strength | 15.0 MPa | 2180 psi | At compression strain of 3%; EN ISO 604 |
Brandenburger BL 70 Slide Bearing Material BL 70 is a low friction material that exhibits stability at high temperatures. Its applications include high-load low friction tracks and linings in transport and conveying systems, high-stressed b.. |