Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2103 MPa | 305000 psi | ASTM C773 |
CoorsTek AD-94 Alumina (nom. 94% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Compressive Strength | 2103 MPa | 305000 psi | ASTM-C773 |
CoorsTek Z-PLUS™ 94 Zirconia-Impr. Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |