Mechanical Properties Metric English Comments
Compressive Strength 142 MPa
20600 psi
ASTM D695
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper..
Compressive Strength 142 MPa
20600 psi
ASTM D695
Plenco 5350 Phenolic, Granular, Compression Molded
PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties...