Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 142 MPa | 20600 psi | ASTM D695 |
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Compressive Strength | 142 MPa | 20600 psi | ASTM D695 |
Plenco 5350 Phenolic, Granular, Compression Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |