Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 14.0 - 20.0 MPa | 2030 - 2900 psi | ASTM D695 |
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st.. |