Mechanical Properties Metric English Comments
Compressive Strength 2.94 MPa
427 psi
Fired at 800°C, Cold Crushing
Sharadaa Ceramics REFINSUL ZAP-018 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..
Compressive Strength 2.94 MPa
427 psi
Fired at Service temp. of 1300°C, Cold Crushing
Sharadaa Ceramics REFINSUL ZAP-015 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..
Compressive Strength <= 2.94 MPa
<= 427 psi
Cold Crushing Strength
Chosun Refractories B-6 Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength <= 2.94 MPa
<= 427 psi
Cold Crushing Strength
Chosun Refractories B-7 Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 MPa

@Temperature 1350 °C,
Time 10800 sec
427 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CC-1 Blast Furnace Tap-Hole Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved