Sharadaa Ceramics REFINSUL ZAP-015 Insulating Castables

Category Ceramic
Manufacturer Sharadaa Ceramics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics REFINSUL ZAP-015 Insulating Castables.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for low density and low thermal conductivity, and are helpful in conserving heat energy thus reducing fuel costs.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density <= 0.900 g/cc
<= 0.0325 lb/in³
Dried at 110°C
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000785 GPa
0.114 ksi
Dried at 110°C
0.000686 GPa

@Treatment Temp. 800 °C
0.0995 ksi

@Treatment Temp. 1470 °F
0.000785 GPa

@Treatment Temp. 1300 °C
0.114 ksi

@Treatment Temp. 2370 °F
Compressive Strength 1.96 MPa
284 psi
Fired at 800°C, Cold Crushing
2.45 MPa
356 psi
Dried at 110°C, Cold Crushing
2.94 MPa
427 psi
Fired at Service temp. of 1300°C, Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity <= 0.232 W/m-K

@Temperature 500 °C
<= 1.61 BTU-in/hr-ft²-°F

@Temperature 932 °F
Component Elements Properties Metric English Comments
Al2O3 >= 40 %
>= 40 %
Fe2O3 <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Permanent Linear Change -0.3 - 0.3%
Fired at 800°C
-1.0 - 1.0%
Fired at Service temp. 1300°C