Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2.55 MPa | 370 psi | 30 g/l |
Jackon JACKOCELL® S232 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S232 which will lead the industry in.. |
|||
Compressive Strength | 2.55 MPa | 370 psi | 30 g/l |
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S332 which will lead the industry in.. |