Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1360 MPa | 197000 psi | ASTM D695 |
Greene Tweed WR™ 525 PEEK, Carbon Filled WR®525 is a thermoplastic composite consisting of carbon fiber in a PEEK matrix. Because of its unique thermal expansion properties, WR525 is deal for use as impeller wear rings, bushings and ca.. |
|||
Compressive Strength | 1360 MPa @Temperature 22.0 °C |
197000 psi @Temperature 71.6 °F |
0° |
Greene Tweed Xycomp® 1001-01 PEEK, Carbon Fiber Filled Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st.. |