Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 134 MPa | 19400 psi | ASTM D695 |
Plenco 08133 Polyester BMC, Compression Molded PLENCO 08133 is a renumber of PlasGlas 10313. PLENCO 08133 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Compressive Strength | 134 MPa | 19400 psi | ASTM D695 |
Plenco 5118 Phenolic, Granular, Compression Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |