Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 12.7 MPa | 1850 psi | Dried at 110°C, Cold Crushing |
Sharadaa Ceramics REFINSUL ZAP-020 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |