Material Notes:
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for low density and low thermal conductivity, and are helpful in conserving heat energy thus reducing fuel costs.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density <= 1.60 g/cc
<= 0.0578 lb/in³
Dried at 110°C
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00235 GPa
0.341 ksi
Dried at 110°C
0.00177 GPa

@Treatment Temp. 800 °C
0.257 ksi

@Treatment Temp. 1470 °F
0.00196 GPa

@Treatment Temp. 1300 °C
0.284 ksi

@Treatment Temp. 2370 °F
Compressive Strength 7.35 MPa
1070 psi
Fired at 800°C, Cold Crushing
8.83 MPa
1280 psi
Fired at Service temp. of 1300°C, Cold Crushing
12.7 MPa
1850 psi
Dried at 110°C, Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity <= 0.511 W/m-K

@Temperature 500 °C
<= 3.55 BTU-in/hr-ft²-°F

@Temperature 932 °F
Component Elements Properties Metric English Comments
Al2O3 >= 43 %
>= 43 %
Fe2O3 <= 1.5 %
<= 1.5 %
Descriptive Properties Value Comments
Permanent Linear Change -0.2 - 0.2%
Fired at 800°C
-1.0 - 1.0%
Fired at Service temp. 1300°C
Copyright © lookpolymers.com All Rights Reserved