Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.24 MPa | 180 psi | 16 hour silo aging time, 20 kg/m^3 |
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |
|||
Compressive Strength | 1.24 MPa | 180 psi | 20 g/l |
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S314 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces ave.. |