Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.120 MPa | 17.4 psi | 16 hour silo aging time, 20 kg/m^3 |
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |
|||
Compressive Strength | 0.120 MPa | 17.4 psi | after 24 hrs at 760°C, as Received, Parallel to Thickness |
Zircar Ceramics ASQ Castertip 14 pcf density refractory ceramic fiber "soft tip". Alumina bonding of shot free fiber results in extreme performance in manufacture of the finest grades of medical, food and packaging foils. Inform.. |