Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 17.2 MPa | 2500 psi | 16%, 0.44 w/c w/Tychem 3000 |
Mallard Creek Polymers Tychem® 3000D Yield Modifier Additive Tychem® 3000/3100D is well suited, but not limited to, dry-cast pavers and blocks, SCC, HPC, pre-cast and down hole cementing. Tychem® 3000/3100D is compatible under the most extreme condition.. |
|||
Compressive Strength | 17.2 MPa | 2500 psi | crush strength |
St. Cloud Natural Zeolite (Clinoptilolite) Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter.. |
|||
Compressive Strength | >= 17.2 MPa | >= 2500 psi | |
Engineered Syntactic Systems SF-25 Subsea Macrosphere Syntactic Void Filler The four part SF-25 kit was developed specifically to meet the critical needs of void space filling at operating pressures to 1000 psi. This system utilizes carbon fiber reinforced epoxy macrosphere.. |
|||
Compressive Strength | 17.2 MPa @Temperature 1350 °C, Time 10800 sec |
2490 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CRS-A60 Blast Furnace Tap-Hole Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |