Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 101 MPa | 14600 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Compressive Strength | 101 - 112 MPa | 14600 - 16200 psi | ASTM D695 |
Cast Nylons Nycast® SLX Premium Bearing Grade Nylon Nycast® SLX closes the gap between static and dynamic coefficients of friction. Used in wear pads, bearing blocks, and other load-bearing slide applications.Data provided by the manufacturer, Cast.. |
|||
Compressive Strength | 101 MPa | 14600 psi | |
Abatron AboCast/AboCure 7606-1 Epoxy AboCast 7606-1 is a transparent, light amber resin with a weight of 9.5 lbs/gallon and a viscosity of 2100 cps approx. @ 25°C. AboCure 7606-1 is a transparent, light amber converter with a weight o.. |