Mechanical Properties Metric English Comments
Compressive Strength 71.0 - 98.6 MPa
10300 - 14300 psi
Bulk Molding Compounds BMC HT12-1024 Automotive Grade Molding compound
BMC HT12-1024 is a high temp wear resistant molding compound designed for automotive brush holders. It is listed under Ford WS-MSD-A. It can be injection or transfer molded.Information provided by..