Polymer Property : Compressive Strength = 1300 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1300 MPa
189000 psi
SGL Carbon Group SIGRAFIL C® in 250°F Epoxy
60% fiber volumeInformation provided by SGL Carbon Group