Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 8.48 MPa | 1230 psi | |
Mo-Sci Corporation GL-0193 Hollow Glass Spheres Appearance: Hollow microspheres with white color in powder form.Applications: GL-0193 is a new, low cost, light weight, hollow glass extender for liquid resin systems offering low cost per unit volu.. |
|||
Compressive Strength | 8.50 MPa @Time 3.60e+7 sec |
1230 psi @Time 10000 hour |
|
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |