Mechanical Properties Metric English Comments
Compressive Strength 6.21 - 8.27 MPa
900 - 1200 psi
@ 1.0% Strain; ASTM D695
Technetics Group Texolon™ 9406 PTFE  (Unverified Data**)
General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel..